ENTHONE 50 Series
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Ambient or Heat-Cure Flexibility
- Multi-Method Permanent Marking
- Chemical- and Thermal-Resistant Films
Product Description
ENTHONE 50-Series Inks are permanent, two-component epoxy screen-printing inks for durable legend and component marking. The family adheres to photoimageable, thermal, and UV solder masks as well as glass, metal, and compatible plastics when properly applied and cured. Catalyst options provide room-temperature or heat-cure processing, while screen printing, spraying, brushing, and roller printing support several marking methods. Cured films provide chemical and thermal resistance, with color-specific electrical insulation data defined for controlled cure and humidity conditions. Applications include circuit boards, semiconductor components, connectors, dials, nameplates, chassis, glass, and thermoplastics.
Key features
- Multiple Marking Methods: Screen printing, spraying, brushing, and roller printing cover varied production requirements.
- Flexible Catalyst Cure: Available catalyst options support room-temperature or controlled heat cure.
- Cured Electrical Characterization: Color-specific insulation resistance is defined before and after humidity conditioning.
Applications / Suitable for
- Permanent circuit-board legends
- Semiconductor-component marking
- Connectors, dials, and nameplates
- Chassis and edge-lit panels
- Glass and thermoplastic marking
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Typical processing data for the ENTHONE 50-Series family. Color- and catalyst-specific conditions are identified where applicable.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Standard catalyst addition | 4.0 to 9.0 | parts by weight | Per 100 parts ink; exact value depends on 50-Series color and catalyst |
| Catalyst 5 addition | 7.0 to 11.5 | parts by weight | Per 100 parts ink; only for colors where Catalyst 5 is recommended |
| Induction period | 30; 60 | min | All standard catalysts; Catalyst 5, respectively |
| Average pot life | 1 to 24 max | hr | Depends on selected catalyst; measured after induction |
| Shelf life | Ink 3; catalysts 2 | years | From date of manufacture |
| Screen mesh | 180 to 350 | mesh count | Monofilament polyester, metallized polyester, or equivalent stainless steel |
| Squeegee hardness | 60 to 80 | durometer | Sharp, nick-free squeegee for screen printing |
After-processing / final-state properties
Typical cured-film data for specified colors and cure conditions. Electrical values vary by ink color and cure schedule.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Recommended cured film thickness | 0.7 to 1.4 (0.017 to 0.035) | mil (mm) | Cured ink film |
| Initial insulation resistance | 50 700R: 1.4 x 10^8; 50 710R: 1.2 x 10^4; 50 770R, 50 771R, and all other colors: >1.0 x 10^12 | ohm | MIL-I-43553A; cured 30 min at 121 deg C |
| Insulation resistance after humidity | 50 700R: 1.7 x 10^8; 50 710R: 1.2 x 10^4; 50 770R, 50 771R, and all other colors: >1.0 x 10^10 | ohm | MIL-I-43553A; 77 +/- 10 deg F and 95% RH for 48 hr; cured 30 min at 121 deg C |
| Low-outgassing cure condition | 30 at 150 | min at deg C | Extended cure for low-outgassing properties |