3M 8992
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- 204 deg C Process Masking
- Clean One-Piece Mask Removal
- Chemical-Process Masking Resistance
Product Description
3M Polyester Tape 8992 is a dark-green polyester masking tape with pressure-sensitive silicone adhesive for high-temperature masking and process protection. The 0.082 mm tape uses a 0.052 mm polyester backing and provides typical adhesion to steel of 48 N/100 mm, tensile strength of 998 N/100 mm, and 148% elongation. The silicone adhesive performs from -50 to 204 deg C, while the polyester construction provides thermal, abrasion, and chemical resistance. The strong backing supports one-piece removal without slivering and leaves a sharp paint line after masking.
Key features
- High-temperature silicone masking: The silicone adhesive performs from -50 to 204 deg C for demanding masking and process exposure.
- Strong one-piece removal: A 998 N/100 mm typical tensile strength supports removal through cured coatings without slivering or breaking.
- Chemical-process masking resistance: Polyester construction and silicone adhesive support masking in anodizing and acid or caustic chemical-milling operations.
Applications
Applications include powder-coat masking, anodizing and chemical-milling masking, composite vacuum-bag holding, flash breaking, and scratch protection during handling and shipping.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Backing | Polyester | Dark green | |
| Adhesive | Silicone | Pressure-sensitive | |
| Backing thickness | 0.052 | mm | ASTM D3652; typical |
| Total tape thickness | 0.082 | mm | ASTM D3652; typical |
| Shelf life | 24 | months | Original packaging; 16 to 27 deg C and 40 to 60% RH |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesion to steel | 48 | N/100 mm | ASTM D3330; typical |
| Tensile strength | 998 | N/100 mm | ASTM D3759; typical |
| Elongation at break | 148 | % | ASTM D3759; typical |
| Temperature use range | -50 to 204 | deg C | Operating range |