3M 7880

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 7880

Main features

  • Dot-Matrix Printable Polyester Facestock
  • Adhesion Across Metals and Plastics
  • Moisture- and Chemical-Resistant Labeling

Product Description

3M Dot Matrix Label Material 7880 is a matte white, topcoated polyester pressure-sensitive label material for dot-matrix printing and handwritten variable information. It uses 3M Adhesive 300 to bond to metals as well as high- and low-surface-energy plastics, while a 55# densified kraft liner provides consistent die cutting during label conversion. The polyester construction is designed for thermal stability and resistance to moisture and chemicals, making it suited to durable identification where printed information and pressure-sensitive attachment must remain legible and secure. Its printable facestock, adhesive system, and conversion liner provide a complete construction for converted industrial label stock.

Key features

  • Dot-matrix printable facestock: The topcoated polyester surface accepts dot-matrix printing and handwriting for variable identification.
  • Broad adhesive substrate range: 3M Adhesive 300 bonds to metals and both high- and low-surface-energy plastics for pressure-sensitive labeling.
  • Thermal and chemical resistance: The polyester label material provides thermal stability with moisture and chemical resistance for durable identification environments.

Applications

Use 3M Dot Matrix Label Material 7880 for durable identification labels, rating plates, variable-data labels, and equipment or electronics labeling that uses converted polyester label stock.

Product Family

3M 7880

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Roll
ColorColor
White
Other Properties
Storage TemperatureStorage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
FacestockTopcoated polyesterMatte white label construction
Print compatibilityDot-matrix printable and hand writableTopcoated facestock
Adhesive3M Adhesive 300 pressure-sensitive acrylicBonds metals and HSE/LSE plastics
Release liner55# densified kraftSupports consistent die cutting

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers